Sign In | Join Free | My himfr.com
Home > Alloy Steel Plates >

AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel

Mianyang Baoheng New Material Technology Co.,Ltd
Contact Now
    Buy cheap AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel from wholesalers
     
    Buy cheap AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel from wholesalers
    • Buy cheap AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel from wholesalers
    • Buy cheap AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel from wholesalers
    • Buy cheap AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel from wholesalers

    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel

    Ask Lasest Price
    Brand Name : ANSTEEL,TISCO,BAOSTEEL,PANGANGGROUP
    Model Number : AISI 660
    Certification : SGS,TUV,BV,ISO,MTC
    Price : Negotiations
    Payment Terms : T/T
    Supply Ability : 50000KGS/Month
    Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-42 days
    • Product Details
    • Company Profile

    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel

    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel


    Description


    Our company provides
    AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.
    All of
    AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar conform to Military standard, nuclear power. 100% Ultrasonic test ASTM E2375 /SAE AMS 2154 /SEP 1923 /GB/T 4162 /EN 10228-3.


    Products Details


    AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar.

    Chemical Composition (weight%):
    C≤ 0.08
    Si≤ 1.00
    Mn≤ 2.00
    P 0.040
    S 0.030
    Cr13.5 ~ 16.0
    Ni24.0 ~ 27.0
    Mo1.00 ~ 1.50
    Ti1.90 ~ 2.35
    Cu≤ 0.025
    Al≤ 0.035
    B0.0010 ~ 0.010
    Mechanical Properties Under Final Heat Treatment:
    Condition / Bar: Solution treated, precipitation hardened
    Tensile strength, σb/≥ MPa950
    Yield strength, σ0.2/≥ MPa650
    Elonghation, δ ≥(%)12.0
    Reduction of area, ф ≥ (%)-
    Hardness | HB-


    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel

    Bars and, where applicable, forgings are subjected to ultrasonic examination based on the different level according to the buyers' requirements.
    The alloy is usually produced by AOD / VIM VOD followed by electroslag refining (ESR) or VAR if necessary for special purpose.
    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade SteelAISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel


    FAQ

    Q: How do you control the quality?

    A: We have professional inspectors to analyze the chemical composition of
    AISI 660 Alloy Steel Plates AISI 660 Black / Bright / Rrough Turned Turbine Blade Steel AISI 660 Round Bar Peeled / Polished AISI 660 Shot blasted / Ground Flat Bar. and test the finished products in strict accordance with the standards stipulated in the contract. In this process, the inner and outer surfaces, the appearance of both ends, bending, set length, outer diameter and Wall thickness will be checked one by one. You can rest assured that all products you receive from us are reliable.


    Q: Do you accept customization?


    A: Yes. If you have special requirements for products or packaging, we can make them for you.


    Q: Can you accept trial orders?


    A: Our MOQ is usually 1 ton. However, if you want to place an order as the start of our cooperation, we can accept smaller quantities at the first time. Of course, after the start, we will have further and longer cooperation.


    Q: How do I get samples?


    A: Free samples are available for your inspection and testing, DHL/FedEx/UPS accounts can be used for sampling, and the courier fee is borne by you.

    AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel


    Submit an enquiry for the displaying steel materials you are interested in TODAY!

    Sales Engineer: sales@ss-bars.com

    Quality AISI 660 Alloy Steel Plates AISI 660 Superalloy Steel Plates AISI 660 Turbine Blade Steel for sale
    Inquiry Cart 0
    Send your message to this supplier
     
    *From:
    *To: Mianyang Baoheng New Material Technology Co.,Ltd
    *Subject:
    *Message:
    Characters Remaining: (0/3000)